When two different metals touch in the presence of moisture, the less noble metal corrodes. Use this free calculator (beta) to check whether a fastener and base metal, such as stainless bolts in galvanized or aluminum framing, are compatible in your environment, which metal will corrode, and how to isolate the joint.
Anodic index values (volts, gold = 0) and allowable differences (0.15 V harsh, 0.25 V normal, 0.50 V controlled) follow the widely published anodic index method. Values are approximate; moisture, temperature, chlorides and the area ratio of the two metals all affect the actual corrosion rate.
Related design tools: Bolt Length Calculator · B8 Class 2 Bolt Torque Calculator · Thermal Washer & Bushing Selector · All engineering design tools
Products: Isolation washers and bushings · Thermal break washers and bushings · B8 Class 2 stainless bolts · Stainless steel fasteners
Need to isolate dissimilar metals? We cut isolation washers, bushings and pads to size and supply stainless fasteners. Call 800-580-4195 or use the form below.